Ok so I tried to weld 035 SS plates together today and it looks terrible between the burn through and poor penetration I did see a little weld that looked good but the back side of the weld looked like crap.
That beeing said what would you guys set a syncrowave 200 at to get good welds and how much tungsten needs ti stick out of the cup?
I have the red tungsten sharpened with a flat point.
tried using about 20 amps on AC PPS at 3.

Help please