    Default MIG Aluminum Porosity ???

    I'm having trouble with porosity. I'm doing a 3/16" deep groove weld in the flat position between 3/16" 6063 and 3/8" 6061 using a 350p and spoolmatic 30a, 4043 .035 wire, pulsing, 50 arc length and about 550 wire speed, pure argon at 30 cfm, prep with stainless brush. The surface looks fine when done welding but when I grind it flush, swiss cheese. Any help would be appreciated.

  2. #2

    Default MIG Aluminum Porosity ???

    Swiss cheese mainly at your start or across the whole weld?

  3. #3

    Default

    It is more pronounced at the starts, but there's some throughout.

  4. #4

    Default MIG Aluminum Porosity ???

    Try cleaning the material with acid or laquer thinner also I find you need a good preflow on the gas

  5. #5
    Join Date
    Sep 2005
    Location
    Salem ,Ohio
    Posts
    3,909

    Cool

    Gun angle. Slightly pushing about 10-15 degrees any more and you will suck in air...Bob
    Bob Wright, Grandson of Tee Nee Boat Trailer Founder
    Metal Master Fab Salem, Oh 44460
    Birthplace of the Silver & Deming Drill
    1999 MM185 w/185 Spoolgun,1986 Thunderbolt AC/DC
    Spool Gun conversion. How To Do It. Below.
    http://www.millerwelds.com/resources...php?albumid=48

  6. #6
    Join Date
    Feb 2013
    Location
    North Dakota
    Posts
    29

    Default MIG Aluminum Porosity ???

    Turn your cfh up to about 45

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  

Warning: Non-static method PhpQuickProfiler::getMicroTime() should not be called statically in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/pqp/classes/Console.php on line 77

Warning: Non-static method PhpQuickProfiler::getMicroTime() should not be called statically in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/pqp/classes/Console.php on line 77

Warning: Non-static method PhpQuickProfiler::getMicroTime() should not be called statically in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/pqp/classes/Console.php on line 77

Warning: Non-static method PhpQuickProfiler::getMicroTime() should not be called statically in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/pqp/classes/Console.php on line 77

Warning: Non-static method PhpQuickProfiler::getMicroTime() should not be called statically in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/pqp/classes/Console.php on line 77

Warning: Non-static method PhpQuickProfiler::getMicroTime() should not be called statically in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/pqp/classes/Console.php on line 77

Warning: Non-static method PhpQuickProfiler::getMicroTime() should not be called statically in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/pqp/classes/Console.php on line 77

Warning: Function split() is deprecated in /mnt/stor3-wc1-dfw1/357822/357839/www.millerwelds.com/web/content/lib/footer.inc.php on line 82

Welding Projects

Special Offers: See the latest Miller deals and promotions.