Does anybody have experience with 4130 chromoly tubing?
I'm going to weld chassis out of .156 wall thickness and I'm wondering if pre and post heating is crucial?
I found on Internet that chromoly tube that are thicker then .120 should be pre and post heated... Thank you for any input...