I am using .023 stainless wire with 75/25% argon /co2 mix. Starts real cold with a lot of spatter and no penetration , then seams to heat up and weld nice but will still go cold mid weld seamingly for no reason. Am I using the right stuff? Is my little 110v mig not running properly?
Results 1 to 8 of 8
Threaded View
-
08-06-2012, 07:14 PM #1
Junior Member
- Join Date
- Aug 2012
- Posts
- 3
I am looking for tips on out of position welding of 16ga stainless.