I had this come up today at work.Another millwright at the plant had to pull the door out of a shot peener and the door is warped.This is a 1/4" thick plate aproximatley 18x24" I believe.It has about a 1" bow in it.
He applied heat to it and put it in a press.He got some of the bow out but not all of it.He was worried about it cracking by taking it too far with the press.
Has anyone here every have any ezperiance with this material?